Material Drying
4 조회수
TPE bubble causes
문제 현상
Bubbles repeatedly appear in TPE products
원인 분석
Bubble causes: the three routes of moisture, degradation, and air entrainment; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry materials and should be confirmed first during troubleshooting
해결 방법
Air-shot identification of the three routes; for moisture check drying, for degradation check temperature, for air entrainment check venting; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes, so as to locate effective measures
핵심 요약
Bubbles are identified and handled by three routes; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems later
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!