Material Drying 4 조회수

TPU drying 0.02% red line

문제 현상
TPU products show bubbles and silver streaks, mechanical properties decline significantly, and products become brittle
원인 분석
TPU is a strongly hygroscopic material and can absorb up to 3% moisture when exposed to air; residual moisture catalyzes hydrolysis in the 180-220℃ melt, breaking molecular chains and reducing molecular weight, manifesting as performance loss and embrittlement
해결 방법
①dehumidify and dry to moisture content ≤0.02% ('2079851475616104452); ②hopper dryer continuously keeps warm to prevent moisture regain; ③use moisture content rather than time as the drying qualification standard
핵심 요약
0.02% is the golden red line for TPU '2079851475616104452; drying to the moisture content specification rather than the time specification is the core proposition of professional manufacturers such as Foster; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
TPU;drying;0.02%;hydrolysis;molecular weight