Material Drying
4 조회수
TPU drying temperature graded by hardness
문제 현상
High-hardness TPU agglomerates and sticks after drying, or low-hardness TPU is under-dried and still has bubbles
원인 분석
TPU drying temperature is graded by hardness: Shore A75-90 uses 80-90℃ (dehumidification) or 100-110℃ (circulating air), Shore A90 and above uses 90-120℃ or 100-120℃; soft material agglomerates at high temperature, hard material does not dry at low temperature
해결 방법
①set the drying temperature graded by hardness; ②for soft TPU prefer low temperature and long time; ③prevent yellowing when drying exceeds 12 hours; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
핵심 요약
TPU drying temperature must match hardness; the higher the hardness the higher the temperature, and a one-size-fits-all parameter will inevitably fail on one side; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!