Internal Shrinkage Porosity in Thick-Walled CPE Products
문제 현상
The center of thick-walled parts is loose or has voids
원인 분석
The center cools slowly and the feeding runner solidifies too early
해결 방법
Optimize gate position and size, extend holding pressure, and increase pressure
핵심 요약
Internal quality of thick-walled parts is a technical difficulty