Molding Process
7 조회수
Filling Difficulty of Long-Flow CPE Products
문제 현상
The far end of large thin-walled products is not fully filled
원인 분석
Long melt flow path, large pressure attenuation, and cooling of the flow front
해결 방법
Multi-gate layout, raise melt temperature, and increase injection speed
핵심 요약
Gate layout is the key
이 정보가 도움이 되었나요?