Injection Molding
5 조회수
Cold slug marks in EAA '2079851475616104452
문제 현상
Cold slug marks appear near the gate of EAA injection molded products
원인 분석
Nozzle temperature too low, residual material from the previous injection cools and solidifies in the nozzle; insufficient cold slug well design, cannot accommodate cold material; insufficient injection pressure
해결 방법
1) Raise the nozzle temperature to 180-240°C; 2) Design a sufficiently large cold slug well in the mold; 3) Ensure fresh melt at the front end of the nozzle before each injection; 4) Increase the injection pressure to push the cold material through the gate
핵심 요약
Cold slug marks are caused by solidified residual material in the nozzle; raising the nozzle temperature and cold slug well design are the key