Injection Molding 5 조회수

EEA injection cold slug marks

문제 현상
Cold slug marks appearing near the gate of EEA injection molded products
원인 분석
Nozzle temperature too low causing residual material from the previous injection to cool and solidify in the nozzle; insufficient cold slug well design unable to accommodate cold material; insufficient injection pressure
해결 방법
1) Increase nozzle temperature to 160-210°C; 2) Mold design with a sufficiently large cold slug well; 3) Ensure fresh melt at the nozzle front end before each injection; 4) Increase injection pressure to push cold material through the gate
핵심 요약
Cold slug marks are caused by solidified residual material in the nozzle; increasing nozzle temperature and cold slug well design are the key
EEA injectioncold slug marksnozzle temperaturecold slug wellinjection pressure