EEA Poor Chemical Resistance
문제 현상
After immersion in acid/alkali solvents, EEA product mechanical properties decline >30%
원인 분석
EEA has high affinity for specific chemicals, being eroded and swollen; EEA molecular chains are attacked by chemicals and broken
해결 방법
1) Select chemical-resistant grades; 2) Slight crosslinking to reduce swelling; 3) Product surface coating protection; 4) Add chemical stabilizers
핵심 요약
Poor chemical resistance is caused by EEA chemical affinity; selecting chemical-resistant grades and coating are key