Processing Machinery 4 조회수

EVA purging is difficult

문제 현상
EVA purging requires 2-3h, time-consuming and affecting changeover efficiency
원인 분석
EVA has strong adhesion, forming a firm adhesive layer on the screw and barrel; EVA has poor thermal stability and becomes sticky at high temperature, making it harder to remove
해결 방법
1) Flush with high-viscosity PE before purging to carry away EVA residue; 2) Reduce purging temperature below the EVA softening point to reduce adhesion; 3) Use a dedicated purging compound
핵심 요약
Purging difficulty is caused by EVA's strong adhesion; PE flushing and temperature reduction are key
EVA purging difficulty adhesion PE flushing dedicated purging compound