EVA foam surface large bubbles
문제 현상
EVA foam large bubbles >2mm
원인 분석
AC locally agglomerated with decomposed large amounts of gas concentrated; foaming temperature too high with local overheating
해결 방법
1) AC masterbatch method to ensure dispersion without agglomeration; 2) Temperature ±2°C; 3) DCP masterbatch method for uniform crosslinking
핵심 요약
Large bubbles are caused by blowing agent agglomeration and uneven temperature; masterbatch method is key