Periodic EVOH Surface Ripples
문제 현상
Periodic ripples with 5-15mm spacing on EVOH product surfaces
원인 분석
Injection speed periodic fluctuation; hydraulic system unstable; screw speed unstable
해결 방법
1) Overhaul injection system to stabilize pressure and speed; 2) Servo motor drive replacing hydraulic drive; 3) PID control to stabilize injection parameters
핵심 요약
Ripples are caused by unstable injection; equipment overhaul and PID control are key