Extrusion & Post
10 조회수
Poor printing adhesion of PU film
문제 현상
After PU film printing, ink adhesion < grade 2, large-area peeling in cross-cut test
원인 분석
PU surface polarity has poor affinity with ink; corona treatment effect decays fast; ink system does not match PU
해결 방법
1) Print immediately after corona treatment within 24h; 2) Use PU-specific ink; 3) Increase corona power to 15-20kW/m² to ensure surface tension >42mN/m; 4) Flame treatment to assist polarizing the surface
핵심 요약
Poor printing adhesion is caused by insufficient surface polarity; corona treatment and special ink are key