Injection Molding 5 조회수

Uneven color when PVA is mixed with color masterbatch

문제 현상
PVA/color masterbatch injection molded products show color streaks and areas of uneven color depth
원인 분석
Color masterbatch carrier resin incompatible with PVA; poor color masterbatch dispersion with pigment agglomeration; unstable melt flow during '2079851475616104452 causes pigment orientation
해결 방법
1) Select PVA or same-type carrier color masterbatch to ensure compatibility; 2) Pre-disperse by twin-screw extrusion granulation; 3) Appropriately extend mixing time to ensure pigment dispersion; 4) Reduce injection speed to reduce pigment orientation
핵심 요약
Color masterbatch carrier matching and full dispersion are the key to color uniformity
PVA coloringcolor masterbatchcarrier compatibilitypigment dispersioncolor streaks