Poor PVA surface gloss
문제 현상
PVA product surface gloss <60%, below the 80% requirement, dull appearance
원인 분석
Mold surface rough Ra>0.4μm; high PVA crystallinity, surface microcrystals scatter light; improper cooling rate
해결 방법
1) Polish mold to Ra<0.1μm mirror finish; 2) Raise mold temperature to delay crystallization and reduce scattering; 3) Add nucleating agent to control crystal size
핵심 요약
Poor gloss is caused by mold roughness and crystallization scattering; polishing the mold and controlling crystallization are the key