Molds & Tooling 4 조회수

Product has sink marks, unstable dimensions, or flash

문제 현상
The product has sink marks, unstable dimensions, or flash, related to the holding pressure setting
원인 분석
Holding pressure insufficient, producing sink marks Holding pressure time too short, insufficient shrinkage compensation Holding pressure too long, stress concentration at the gate area Holding pressure switchover too early, dimension fluctuation Holding pressure too high, flash
해결 방법
Increase holding pressure to 80-120MPa Holding pressure time 15-30s, according to gate freezing time Reasonably set the holding pressure switchover point Avoid excessive holding pressure producing flash Adjust holding pressure according to the cellulose acetate butyrate shrinkage rate 0.4-0.6%
핵심 요약
Holding pressure needs to be set according to shrinkage rate and gate freezing time
holding pressureshrinkage compensationshrinkage rategate freezing