Material Drying 4 조회수

Insufficient bonding force between metal layer and substrate after CAB product electroplating

문제 현상
Insufficient bonding force between the metal layer and the substrate after CAB product electroplating, plating peels off or blisters
원인 분석
Insufficient CAB surface roughening treatment Improper cleaning or activation process before electroplating High CAB moisture content affects roughening effect Electroplating solution formula not matching CAB Improper roughening time or temperature
해결 방법
Optimize the roughening treatment process to ensure sufficient surface roughening Improve cleaning and activation steps before electroplating Fully dry CAB to reduce moisture Select electroplating solution matching CAB Control roughening time and temperature
핵심 요약
CAB electroplating requires optimizing roughening and activation processes