Molds & Tooling 4 조회수

Runner cross-section, length, and layout design unreasonable

문제 현상
Runner cross-section, length, and layout design unreasonable
원인 분석
Runner cross-section too small, large resistance, difficult filling Runner too long, large pressure loss, short shots at the end Unbalanced runner layout, filling differences between cavities Improper runner cold slug well design, cold slug enters the cavity Unsmooth transition between runner and gate, producing turbulence
해결 방법
Increase runner cross-section to reduce resistance Shorten runner length to reduce pressure loss Balance runner layout to ensure uniform filling of each cavity Reasonably design cold slug wells to prevent cold slug Smooth transition between runner and gate
핵심 요약
Runners need balanced layout and appropriate cross-section
runner designcross-sectionlayoutcold slug well