CEF hardness too low
문제 현상
The Shore hardness of the CEF product is 5-10 degrees lower than the target and feels soft
원인 분석
The soft nature of CEF has low hardness; too much plasticizer or softener is added; the crystallinity is low
해결 방법
1) Add rigid filler 5-10wt% to increase hardness; 2) Reduce the amount of plasticizer; 3) Increase the cooling rate to increase the crystallinity
핵심 요약
Low hardness is caused by the softness of the material and excessive plasticization; adding fillers is the key