Injection Molding
5 조회수
Insufficient Flow Length Ratio in CMC '2079851475616104452
문제 현상
CMC '2079851475616104452 flow length ratio is only 80-100, lower than 150, and thin-walled products cannot be filled
원인 분석
CMC melt viscosity is high and flow distance is short; injection temperature is low; injection pressure is insufficient; mold runner resistance is large
해결 방법
1)Increase injection temperature to 20-25°C; 2)Increase injection pressure 80-100MPa; 3)Enlarge runner and gate sizes to reduce resistance; 4)Add 0.3-0.5wt% flow aid to reduce viscosity
핵심 요약
Insufficient flow length ratio is caused by CMC high viscosity; high temperature, high pressure and large gate are the key