Poor Weather Resistance of CMC
문제 현상
After 6 months outdoors, CMC mechanical properties decrease by 40-50% and the surface cracks
원인 분석
Photo-oxidative degradation of the CMC polyolefin backbone breaks molecular chains; ultraviolet rays directly attack C-C bonds
해결 방법
1)UV-327 0.5-1wt% to absorb ultraviolet rays; 2)HALS-770 0.2-0.5wt% for light stabilization; 3)1010+168 antioxidant 0.3wt% to prevent oxidation
핵심 요약
Poor weather resistance is caused by photo-oxidation; UV+HALS+antioxidant triple protection is the key