Material Analysis 11 조회수

Poor interfacial bonding between DSTDP and filler

문제 현상
The tensile strength of the DSTDP/filler composite is instead lower than that of pure DSTDP, playing a negative role
원인 분석
The interfacial affinity between filler and DSTDP is poor and no coupling agent treatment was used; filler particles agglomerate with dispersed particle size >5μm; DSTDP has insufficient wettability to rigid fillers
해결 방법
1) Filler pretreatment: treat with silane coupling agent KH-560 at 0.5-1wt%; 2) add DSTDP compatibilizer 2-3wt% to strengthen interfacial bonding; 3) use ultrafine filler d50<2μm; 4) twin-screw high-shear compounding to ensure dispersion
핵심 요약
The elastomer-filler interface requires the dual action of coupling agent and compatibilizer, otherwise the filler plays a negative effect
DSTDP fillerinterfacial bondingcoupling agentcompatibilizerfiller dispersion