Glass Fibre poor weather resistance
문제 현상
Glass Fibre after 6 months outdoors mechanical properties drop 40-50%, surface cracking
원인 분석
Glass Fibre polyolefin backbone photo-oxidative degradation, molecular chains break; ultraviolet directly attacks C-C bonds
해결 방법
1) UV-327 0.5-1wt% absorbs ultraviolet; 2) HALS-770 0.2-0.5wt% light stabilization; 3) 1010+168 antioxidant 0.3wt% prevents oxidation
핵심 요약
Poor weather resistance is caused by photo-oxidation; UV+HALS+antioxidant triple protection is key