Injection Molding
5 조회수
MP '2079851475616104452 difficult demolding
문제 현상
MP injection molded products have large demolding force, products deformed or scratched, demolding time accounts for 30% of the cycle
원인 분석
MP has large adhesion to the mold cavity; draft angle insufficient <0.5°; cooling time insufficient, product demolded before fully solidified; ejection mechanism design unreasonable
해결 방법
1) increase mold draft angle to 1-2°; 2) extend cooling time so the product is fully solidified before demolding; 3) polish mold surface to Ra<0.2μm; 4) increase ejection area using a large-area ejector plate; 5) spray mold release agent (temporary solution)
핵심 요약
difficult demolding is caused by adhesion and insufficient mold design; increasing the draft angle is the fundamental measure
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!