Material Analysis 11 조회수

MP product dimensional change during long-term storage

문제 현상
MP products after 3 months of storage have dimensional change ±2-3%, exceeding the ±0.5% requirement
원인 분석
MP physical aging relaxation causes continuous dimensional change; secondary crystallization slowly changes density and dimensions; low molecular species slowly migrate changing local density
해결 방법
1) anneal products at 80°C/4h before leaving the factory to stabilize dimensions; 2) select high molecular weight grades to reduce low molecular species; 3) slight crosslinking to reduce molecular chain mobility and inhibit aging; 4) control storage environment temperature at 23±2°C to reduce temperature change effects
핵심 요약
dimensional change is caused by physical aging; annealing and slight crosslinking are measures to stabilize dimensions
MP dimensional stability physical aging annealing secondary crystallization slight crosslinking