MP surface dense pitting
문제 현상
MP product surface has dense 0.1-0.3mm pits, affecting appearance and coating adhesion
원인 분석
raw material contains impurity particles >0.05%; mold cavity surface damaged or corroded pits
해결 방법
1) replace with pure raw material, impurities <0.01%; 2) repair and polish the mold cavity to Ra<0.2μm; 3) filter the raw material to remove particles
핵심 요약
pitting is caused by raw material impurities and mold damage; pure raw material and mold maintenance are key