문제 현상
MP product Shore hardness 5-10 degrees higher than the target, hard to the touch
원인 분석
MP crystallinity high, rigidity increased; filler added too much; cooling too fast, crystallization incomplete but rigidity frozen
해결 방법
1) reduce cooling rate to complete crystallization and reduce the hard feel; 2) reduce filler addition; 3) add plasticizer 0.5wt% to lower hardness
핵심 요약
high hardness is caused by crystallization and filler; adjusting cooling and filler are key