Control of appearance abnormality in PEOX hot pressing water-soluble bags
문제 현상
During PEOX hot pressing production of water-soluble bags, the problem of uneven appearance occurs.
원인 분석
Mainly due to the processing temperature deviating from the window +60-100°C, moisture content >0.5% exceeding the standard, and shear heat accumulation.
해결 방법
Strictly control the temperature within the recommended range, fully dry the material to moisture content <0.1%, and shorten the residence time.
핵심 요약
PEOX processing requires precise control of the three elements of temperature, humidity, and residence time.