PC/ABS product surface silver streaks
문제 현상
Silver streaks appear on the surface of PC/ABS products.
원인 분석
The PC component is sensitive to moisture; with insufficient drying and moisture >0.04%, PC hydrolyzes during processing to produce gas, forming silver streaks.
해결 방법
Dry at 80-95°C for 4-6h to moisture <0.04%, dew point ≤-30°C.
핵심 요약
PC/ABS drying is the first checkpoint of surface quality.