POE hardness too high
문제 현상
POE product Shore hardness 5-10 degrees higher than target, hard hand feel
원인 분석
POE crystallinity too high, rigidity increased; too much filler added; cooling too fast, crystallization incomplete but rigidity frozen
해결 방법
1) Reduce cooling rate to make crystallization complete and reduce hard feel; 2) Reduce filler addition; 3) Add plasticizer 0.5wt% to reduce hardness
핵심 요약
High hardness is caused by crystallization and filler; adjusting cooling and filler is key