7 조회수
Filling difficulty of TPU long-flow products
문제 현상
The far end of large thin-walled products is not fully filled
원인 분석
The melt flow path is long, the pressure attenuation is large, the flow front cools
해결 방법
Multi-gate arrangement, raise the melt temperature, increase the injection speed
핵심 요약
Gate layout is the key