Molding Process
4 조회수
Low processing temperature causes poor plasticization
문제 현상
Below 220C, plasticization is insufficient and the surface is rough
원인 분석
The temperature is low, the material is not fully melted, and plasticization is insufficient
해결 방법
Raise to the reasonable range of 220-260C
핵심 요약
The processing temperature window determines plasticization