Injection Molding
4 조회수
Core shift of general-purpose polyethylene injection mold causing uneven wall thickness
문제 현상
The wall thickness of the product is thick on one side and thin on the other, and in severe cases penetration occurs.
Core shift leads to uneven wall thickness, affecting the product strength and dimensional accuracy, and is common in long cores and slender products.
원인 분석
(1)The core is slender and has insufficient rigidity, and bends and shifts under the action of melt pressure
(2)The gate position is improper, and single-side feeding generates lateral unbalanced pressure
(3)The core support is insufficient or the fixing is not firm
(4)The injection pressure is too high or the injection speed is too fast, and the impact force of the melt on the core is large
(5)The fitting clearance between the core and the cavity is too large
해결 방법
(1)Optimize the core design, increase the cross-section of the core root or use high-strength mold steel
(2)Adjust the gate position, and use symmetrical multi-point gates to make the melt fill the mold uniformly
(3)Strengthen the core support structure to ensure that the core is firmly fixed
(4)Appropriately reduce the injection pressure and injection speed to reduce the impact on the core
(5)Control the fitting clearance between the core and the cavity within 0.02mm
핵심 요약
Core shift is caused by insufficient rigidity or uneven force, and needs to be solved from core design, gate layout, and injection parameters.