Extrusion & Post 4 조회수

Unstable output/surging in heat-resistant polyethylene extrusion process

문제 현상
The extruder output is sometimes more and sometimes less, the extrudate is uneven in thickness, and periodic surging occurs. Unstable output directly affects product dimensional accuracy and quality consistency.
원인 분석
(1) Screw feeding section conveying unstable, solid bed breaks (2) Hopper feeding not smooth, raw material bridges (3) Barrel temperature setting improper, feeding section temperature too high or too low (4) Screw rotation speed fluctuates (5) Raw material particle size uneven or too much powder contained
해결 방법
(1) Optimize barrel temperature distribution, appropriately reduce feeding section temperature to prevent premature melting (2) Install a vibrator on the hopper to prevent bridging and ensure continuous feeding (3) Reasonably set the temperature of each barrel section to ensure it is within 190-230°C (4) Check the extruder drive system, stabilize screw rotation speed (5) Control raw material particle uniformity, powder proportion not exceeding 5%
핵심 요약
Unstable output is caused by unstable solids conveying, and the barrel temperature and feeding system need to be optimized.
unstable outputsurgingsolids conveyinghopper bridgingscrew rotation speed