메뉴
재료 기계
인사이트
기사 동영상 문제 및 해결책
About
Chembull 소개 미디어 파트너
문의하기
언어
EnglishالعربيةPortuguêsEspañolDeutschTürkçe한국어
문제 및 해결책으로 돌아가기
Production & Quality 4 조회수

Unreasonable die head flow channel design of heat-resistant polyethylene extruder

문제 현상
The flow velocity of the extrudate is uneven at various parts, and the cross-sectional dimensional deviation of the product is large. Die head flow channel design directly affects the uniformity and quality of the extrudate.
원인 분석
(1) Unreasonable die head flow channel distribution, unequal flow path lengths at various parts (2) Die sizing section length insufficient (3) Dead corners in flow channel, material stagnates and degrades (4) Flow channel surface finish insufficient (5) Die head heating uneven
해결 방법
(1) Optimize flow channel design, use coat-hanger or manifold distributors to ensure equal flow path lengths (2) Increase die sizing section length to stabilize melt flow (3) Eliminate flow channel dead corners, all corners transition with arcs (4) Polish flow channel surface to Ra≤0.2μm (5) Optimize die head heating ring layout to ensure uniform temperature
핵심 요약
Die head flow channel design needs to ensure uniform melt distribution and no material stagnation, and the die head should be redesigned when necessary.
die head flow channeluniform flow velocitysizing sectionflow channel dead cornertemperature uniformity

이 정보가 도움이 되었나요?

0 명이 도움이 되었다고 합니다