Melt flow rate mismatch of raw material for polyolefin plastomer extrusion (Variant: strengthened measures)

문제 현상
After using a certain batch of raw material, the extrusion process parameters need to be greatly adjusted and product quality fluctuates. MFR mismatch makes the original process parameters inapplicable, affecting production efficiency. Especially on the original basis, additional attention is needed, and this problem is more prominent and requires key attention.
원인 분석
(1) Raw material MFR too low, high extrusion energy consumption and low output (2) Raw material MFR too high, product mechanical properties decrease (3) Different grades of raw materials mixed, MFR inconsistent (4) Raw material stored too long, MFR changes (5) Large batch-to-batch MFR fluctuation of raw material (6) On the original basis, additional attention is needed: process parameter fluctuations or equipment state changes aggravate this problem
해결 방법
(1) Select extrusion grades with suitable MFR, polyolefin plastomer extrusion usually selects MFR 0.3-5g/10min (2) Test MFR of each batch of raw material to match process requirements (3) Avoid mixing different grades, test first if mixing is necessary (4) Use raw materials within the shelf life (5) Appropriately increase barrel temperature when MFR is low (6) Appropriately reduce barrel temperature when MFR is high (6) And strengthen process monitoring; on the original basis, additional attention is needed, paying special attention to parameter stability
핵심 요약
MFR mismatch needs to be solved by selecting suitable grades and adjusting temperature parameters. Targeted preventive measures need to be taken in different production scenarios.