문제 현상
The product is plasticized unevenly, the output is low or the energy consumption is high, and the screw does not match the raw material characteristics. The screw design directly affects plasticization quality, output, and energy consumption.
원인 분석
(1) The screw compression ratio does not match the density and melting characteristics of polypropylene (2) The screw length-to-diameter ratio is insufficient, and the plasticizing section length is not enough (3) The transition section between the screw tip and the die head is designed improperly (4) The screw mixing elements are not suitable for this material (5) The screw flight depth is designed improperly
해결 방법
(1) Select a screw compression ratio suitable for polypropylene, generally 2.5-4.0 (2) The screw length-to-diameter ratio is at least 25:1 to ensure full plasticization (3) Optimize the transition section between the screw tip and the die head to eliminate stagnant material areas (4) Select suitable mixing elements (pins, barriers, etc.) according to the material characteristics (5) Ask professional screw designers to optimize the thread parameters according to the material characteristics
핵심 요약
The screw design needs to match the material characteristics and product requirements, and a special screw needs to be customized when necessary.
screw designcompression ratiolength-to-diameter ratiomixing elementscrew matching

이 정보가 도움이 되었나요?

0 명이 도움이 되었다고 합니다

ChemAI