Extrusion & Post 12 조회수

Poor transparency of homopolymer polypropylene blown film

문제 현상
Film haze is high, transparency does not meet requirements. Poor transparency affects product appearance and display effect, especially important in packaging film and optical film.
원인 분석
(1) High crystallinity of homopolymer polypropylene; crystalline regions scatter light causing high haze (2) Melt temperature too low, insufficient plasticization (3) Slow cooling rate, high crystallinity (4) Impurities or gels in raw material (5) Rough film surface
해결 방법
(1) Appropriately increase extrusion temperature to the higher value within the 200-280°C range, full plasticization (2) Improve air ring cooling efficiency, speed up cooling to reduce crystallinity (3) Select grades with good transparency or add nucleating agents to refine grains (4) Strengthen filtration, use 80-120 mesh filter screens to remove impurities (5) Polish the die, improve film surface finish
핵심 요약
Poor transparency is caused by high crystallinity or impurities; it needs to be improved by increasing temperature, speeding up cooling, and selecting appropriate materials.
poor transparencycrystallinitycooling ratenucleating agenthaze