Material Drying
3 조회수
Delamination of PET barrier bottles
문제 현상
Interlayer peeling occurs in multi-layer co-injected PET barrier bottles (containing EVOH, etc.), and barrier performance is lost.
원인 분석
Poor interlayer adhesion; material temperature windows do not match; insufficient drying of the middle layer produces gas; shear differences cause interface instability.
해결 방법
Use compatibilizers or adhesive layers; optimize the processing temperature of each layer to match viscosities; ensure each layer is fully dried.
핵심 요약
The interlayer bonding force of PET multi-layer bottles is the foundation of barrier performance.