Extrusion & Post 7 조회수

Carbonization in PET waste yarn recycling and granulation

문제 현상
During PET waste yarn recycling and granulation, the material carbonizes and turns black, producing black particles and a burnt smell.
원인 분석
The waste yarn contains a large amount of spinning oil agent that degrades and carbonizes at high temperature; extrusion temperature is on the high side; waste yarn bulk density is low and feeding is uneven.
해결 방법
Pre-wash the waste yarn to remove surface oil agents; use a forced feeding device; reduce extrusion temperature; use a vented extruder.
핵심 요약
PET waste yarn recycling requires pretreatment to remove oil agents to prevent extrusion degradation.
PETwaste yarn recyclingcarbonizationoil agentforced feeding