4 조회수
Poor weather resistance of PLA, outdoor decomposition
문제 현상
PLA embrittles and decomposes after 1-3 months of outdoor use.
원인 분석
The combined action of outdoor ultraviolet rays, moisture, and temperature causes PLA to degrade rapidly.
해결 방법
Restrict outdoor use; if outdoor use is necessary, a composite light-resistant and waterproof protective layer is required.
핵심 요약
PLA is not suitable for long-term outdoor use.