Material Analysis 4 조회수

Transparency of polyamide 410 (bio-based long carbon chain nylon) Significantly Decreased After Modification

문제 현상
The transparency of polyamide 410 (bio-based long carbon chain nylon) significantly decreases after modification, the haze increases, and it does not meet the requirements of transparent products
원인 분석
The refractive index of the added additive does not match that of polyamide 410 (bio-based long carbon chain nylon) The additive is unevenly dispersed, producing scattering The processing temperature is too high, and the additive degrades and discolors The amount added is too large, affecting the transparency The change in crystallinity affects the transparency
해결 방법
Select an additive with a matching refractive index Ensure the additive is evenly dispersed Control the processing temperature to avoid additive degradation Reduce the amount added Control the crystallization conditions
핵심 요약
The decrease in transparency needs to be addressed from refractive index matching and dispersion
transparencyhazerefractive indexdispersion