Injection Molding
4 조회수
Tiger skin patterns on product surface
문제 현상
The surface shows regular or irregular tiger skin-like textures
원인 분석
Melt flow in the cavity is unstable (elastic turbulence); the injection speed curve fluctuates; improper gate design causes a transition from jetting to laminar flow
해결 방법
Optimize the multi-stage injection speed control curve; use appropriate gate type and size; increase mold temperature to slow melt cooling
핵심 요약
Tiger skin patterns are a macroscopic manifestation of flow instability
이 정보가 도움이 되었나요?
0 명이 도움이 되었다고 합니다
의견 주셔서 감사합니다!