일반적인 플라스틱 재료 문제에 대한 실질적인 답변

11636 질문
Q
PP Injection Multi-cavity Imbalance
A
For multi-cavity imbalance, first measure filling balance.
Injection Molding PP;multi-cavity;balance;runner;valve gate
Q
PP Injection Part Weld Line Whitening
A
White weld line = cold front + gas and impurity enrichment.
Injection Molding PP;weld line;whitening;venting;overflow well
Q
PP Part Surface Ripple (Flow Mark)
A
Ripple = disordered front rhythm—smooth out the speed profile.
Molds & Tooling PP;ripple;melt front;speed profile;mold temperature
Q
PP Injection Part Short Material—Poor Venting Type
A
Repeated fixed-point shortage = poor venting—locate with the short shot method.
Injection Molding PP;material shortage;venting;short shot method;gate
Q
PP Part Stress Crack Resistance
A
Verify ESCR before holding chemicals.
Production & Quality PP;ESCR;stress cracking;media;grade
Q
PP '2079851475616104458 Webbing
A
For olefin sheet '2079851475616104458, make good use of pre-blow bubbles to prevent webbing.
Thermoforming PP;'2079851475616104458;webbing;pre-blow bubble;TPO
Q
PP-R Pipe Extrusion Rough Surface
A
For rough surface, check temperature and raw material first.
Extrusion & Post PP-R;pipe;rough surface;temperature;raw material