일반적인 플라스틱 재료 문제에 대한 실질적인 답변

11636 질문
Q
Uneven Wall Thickness of LDPE Blow Molded Bottles
A
The wall thickness program is the core.
Blow Molding LDPE; '2079851475616104457; uneven wall thickness; parison program; drop
Q
Poor Surface Gloss of LDPE Injection Molded Products
A
Soft material gloss relies on mold temperature and polishing.
Injection Molding LDPE; '2079851475616104452; gloss; mold temperature; polishing
Q
LDPE Film Slip Agent Blooming
A
Blooming = excessive additive precipitation.
Extrusion & Post LDPE; film; blooming; slip agent; precipitation
Q
Fast Pressure Differential Rise of LDPE Extrusion Filter Screen
A
Fast pressure differential rise = dual sources of gel + impurities.
Extrusion & Post LDPE; extrusion; filter screen; gel; regrind
Q
LDPE Film Winding Edge Wandering
A
Edge wandering = joint action of tension + thin-thick edges.
Extrusion & Post LDPE; film; winding; edge wandering; tension
Q
LDPE Injection Molded Product Deformation - Ejection Type
A
Soft material ejection needs 'fully cooled + large area'.
Injection Molding LDPE; '2079851475616104452; ejection deformation; cooling; ejection
Q
Rough Surface of LDPE Blow Molded Bottles
A
2079851475616104457 surface = parison temperature + blow air energy.
Blow Molding LDPE; '2079851475616104457; rough surface; blow air pressure; mold temperature
Q
Burnt Material at LDPE Extrusion Die Head
A
Burnt material = dead-spot stagnation degradation.
Extrusion & Post LDPE; extrusion; burnt material; die head dead spot; degradation
Q
Stress Cracking of LDPE Injection Molded Products
A
Soft materials also fear long-term overstress.
Injection Molding LDPE; stress cracking; interference; creep
Q
Unstable Frost Line in LDPE Blown Film
A
The frost line is the thermometer of the blown film process.
Extrusion & Post LDPE; blown film; frost line; air ring; crystallization