Extrusion & Post
6 görüntüleme
ABS FDM printing temperature
Sorun Belirtisi
[Problem phenomenon] ABS filament printing warpage and layer cracking, improper parameters
Neden Analizi
ABS FDM nozzle 230-250°C, bed temperature 100-110°C, enclosed chamber to prevent warpage; low temperature causes weak interlayer, high temperature causes degradation and strong odor
Çözüm
Nozzle 230-250°C, bed temperature 100-110°C; enclosed chamber; less fan cooling; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Temel Çıkarım
ABS printing 230-250°C with enclosed chamber to prevent warpage; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for subsequent similar problems