Material Drying
5 görüntüleme
ABS weld line bubble
Sorun Belirtisi
[Problem Phenomenon] ABS bubbles gathering at weld line
Neden Analizi
Convergence entraps air plus venting end effect; more obvious when moisture not fully removed; during on-site troubleshooting, verify item by item according to this mechanism, avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry materials and should be confirmed first during troubleshooting
Çözüm
Strengthen venting in weld line area; drying up to standard; convergence position optimization; after adjustment, continuously sample to verify the effect, resume mass production only after confirming stability; change only one variable each time and record parameter changes to facilitate locating effective measures
Temel Çıkarım
For ABS weld line bubbles check venting and drying; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems later
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu