Production & Quality 5 görüntüleme

ASA tensile strength 48MPa

Sorun Belirtisi
ASA tensile yield strength 48MPa, mechanical performance management.
Neden Analizi
ASA tensile yield strength 48MPa; tensile yield strain 3.3%; elongation at break 9%; flexural strength 70MPa; ball indentation hardness 80MPa; mechanical performance; application matching.
Çözüm
①Mechanical performance testing; ②application matching; ③strength management; ④hardness verification; ⑤quality control.; After adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
Temel Çıkarım
ASA mechanical performance is the application foundation; testing ensures quality; matching ensures function.; After confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
ASA;tensile strength;48MPa;flexural;hardness;testing