ASA heat deflection 101°C

Sorun Belirtisi
ASA heat deflection temperature 101°C annealed, heat resistance management.
Neden Analizi
ASA heat deflection temperature 101°C (annealed 0.45MPa); Vicat softening 97°C; heat resistance performance; application temperature; long-term stability; grade differences.
Çözüm
①Heat deflection 101°C reference; ②application temperature evaluation; ③long-term stability; ④grade selection; ⑤heat resistance verification.; After adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
Temel Çıkarım
ASA heat deflection temperature is a heat resistance indicator; application evaluation ensures safety; verification ensures long-term.; After confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
ASA;heat deflection;101°C;Vicat;heat resistance;stability