HDPE product ESCR stress cracking

Sorun Belirtisi
HDPE containers crack after holding detergents and oils for a period of time.
Neden Analizi
HDPE is prone to environmental stress cracking in media such as surfactants; it starts first at areas with high internal stress, and the ESCR resistance of grades varies greatly.
Çözüm
①Select ESCR-resistant grades according to the medium (high MFR control/comonomer modification); ②reduce product internal stress; ③conduct medium immersion verification; ④avoid sharp corners and interference fit assembly.
Temel Çıkarım
HDPE holding chemicals, ESCR verification cannot be skipped.
HDPE; ESCR; stress cracking; medium; grade