Extrusion & Post
5 görüntüleme
HDPE film poor transverse tear
Sorun Belirtisi
The transverse tear strength of the film is low, unbalanced with the longitudinal performance.
Neden Analizi
Insufficient blow-up ratio makes the transverse molecular chains insufficiently stretched; uneven discharge from the die gap also causes dispersion of transverse performance.; when troubleshooting on site, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
Çözüm
①Increase the blow-up ratio to 2~4 times; ②balance the biaxial draw ratios; ③check the discharge uniformity of the die gap; ④adjust the resin structure if necessary.; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Temel Çıkarım
The balance of transverse and longitudinal performance depends on the matching of blow-up ratio and draw ratio; biaxial testing is the direct method to verify the balance.; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu
Geri bildiriminiz için teşekkürler!